软 – 邵氏2A硬度,使用更少的SLACKER®触变剂,用于比较软的应用场合
低粘度 - 长时间的工作时间,可以减少气泡并使浇注更容易
固化干燥 - 不会析出硅油
长工作时间 - 10-12分钟的工作时间适用于较大的浇注或注射
快速固化 - 40分钟固化时间可以快速旋转浇注或模具
更加可行 - 做更多 - 有“凝胶”阶段 - 将材料塞入假体模具更容易
Before you begin, pre-mix Part B thoroughly. After dispensing required amounts of Parts A and B into mixing container (1A:1B by volume or weight), mix thoroughly making sure that you scrape the sides and bottom of the mixing container several times.
For best results, pour your mixture in a single spot at the lowest point of the containment field. Let the rubber seek its own level. A uniform flow will help minimize entrapped air. If using as a mold material, the liquid rubber should level off at least 1/2” (1.3 cm) over the highest point of the model surface.
Allow rubber to cure for 45 minutes at room temperature (73°F / 23°C) before demolding. Time to demold can be reduced with mild heat or by adding an appropriate amount of Plat-Cat® cure accelerator (See Plat-Cat® technical bulletin available at www.smooth-on.com for details). The pot life and cure times can be extended using Slo-Jo® cure retarder (see Slo-Jo® technical bulletin available at www.smooth-on.com for details). Do not cure rubber where temperature is less than 65°F / 18°C.