ER 205还可用于环氧树脂、聚氨酯树脂以及热塑性塑料脱模。EASE RELEASE 205可用于各种基材,包括钢、铝、铬、环氧树脂、聚氨酯橡胶和塑料、密封膏、封闭的混凝土和蜡。
特征
易于使用
快干
在70°F至500°F的宽温度范围内有效
优异的脱模性
不会干扰细节复制
哑光效果
说明
Model Preparation – if making molds using urethane or silicone rubber, the model surface may need to be sealed (using a sealing agent) before applying release agent. Read the technical bulletin for the mold rubber you are using before proceeding.
APPLYING EASE RELEASE 205 Safety First – Do not smoke or use ignition sources when using sealing or release agents. Use only with good ventilation. Store and use at room temperature.
Shake well before using
Hold spritzer pump 6 in./ 15 cm. from surface to be sprayed.
Apply a light mist coating to all surfaces that will contact the rubber or casting material including model or mold surface and surrounding forms. DO NOT OVER APPLY.
Using a soft brush, brush the release agent over all surfaces. Allow to dry for 10 minutes.
Important - this product has a limited shelf life and should be used as soon as possible.
Ease Release 205 is available in an easy-to-use aerosol called Ease Release 200. For additional information, safety recommendations, or technical assistance please contact us at 610.252.5800.
AVAILABILITY - EASE RELEASE 205, along with the entire line of release agents and mold cleaners, are available through our network of quality distributors located throughout the world.
CAUTION - Use adequate protection when handling any release solvent system. Skin contact may cause dryness. Wear safety glasses or their equivalent to prevent eye injury. Avoid inhalation of excessive amounts of solvent vapor. Do not smoke or use ignition sources when using any solvent system. Always consult Material Safety Data Sheet before using any sealer or release agent.