Epic® Epoxy Thinner

Epic® Epoxy Thinner

Epic®环氧稀释剂为透明、水状液体,可降低Smooth-On浇注和层压环氧树脂的粘度。Epic®可以不同比例添加到环氧树脂系统中,提高流动性,使其更容易混合和浇注。Epic®还有助于减少气泡包裹。
 
Epic®环氧稀释剂不是溶剂,无危害、不含VOC或邻苯二甲酸盐。通常用于稀释环氧树脂的溶剂会导致收缩。Epic®是100%反应性流体,不蒸发,不会导致收缩。Epic®还有助于提高填料的填充量并提供更好的润湿性和浸渍性。

特征

说明

PREPARATION - Store and use all materials at 73°F / 23°C. Avoid breathing fumes - use in a well ventilated area at minimum. NIOSH approved respirator is recommended. Wear safety glasses, long sleeves and rubber gloves to minimize skin contact.
 

USAGE - Epic® Thinner is added by weight. A gram scale is required. Read and follow directions given on the technical bulletin for the EpoxAcast® or EpoxAmite® product before adding Epic® Thinner.

Important - Physical and performance properties (including Shore hardness) of cured epoxy system may be lower in proportion to the amount of Epic Thinner added. Do not exceed recommended loading maximum of 10% of epoxy Part A, as the epoxy system may not cure. A small scale test is recommended if outcome is uncertain.

MEASURING AND MIXING - Add Epic® Thinner to Part A of the epoxy system and pre-mix thoroughly before adding Part B. Mix all parts thoroughly and apply. Usage Example - Epic® Epoxy Thinner and EpoxAmite® 100 with 101 Hardener 100g EpoxAmite 100 (Part A) + 5g Epic® Thinner (Mix Thoroughly) + 24g EpoxAmite® 101 Hardener (Part B) = Viscosity: 900 cps Shore Hardness: 84D