Silicone Thinner®

Silicone Thinner®

有机硅稀释剂是一种非反应性硅油,可降低锡固化(缩合聚合)或铂金固化(加成)硅胶产品的混合粘度。
 
 
有机硅稀释剂具有以下优点:
较低的混合粘度(A + B)意味硅胶在抽真空时会更快地脱气
混合硅胶(A +B)在复杂的模型细节上流动性更好
有机硅稀释剂会降低固化硅胶的最终邵氏硬度(硬度)
操作时间(工作时间)随有机硅稀释剂使用量的增加而延长。
缺点:最终的撕裂强度和拉伸强度与有机硅稀释剂的添加量成比例地降低,但MoldMax®系列橡胶的多节撕裂特性不受影响

特征

说明

Materials should be stored and used in a warm environment (73° F / 23° C). This material has a limited shelf life and should be used as soon as possible. Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk.
 

*Silicone Thinner® is added as a percentage of the total Part A+Part B rubber system. An accurate gram scale must be used. Weigh out and pre-mix required amount of Silicone Thinner® with Part A of silicone rubber before adding Part B. Mix all components thoroughly and vacuum as directed on mold rubber technical bulletin.

It is not recommended to exceed 10% by weight of total system (A+B).

Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.