Sherri Haab is a best selling craft author with over 20 published books to her credit, with several selling over a million copies each. Award winning titles such as: The Art of Resin Jewelry and Designer Style Jewelry (Watson Guptill). Publishing honoraries include Craftrend’s 2006 & 2007 Best General Craft Book Award, Publishers Weekly Cuffie Award, and Oppenheims Toy Portfolio Gold Award. She has recently released a how-to DVD about Resin Jewelry. Television appearances include: The Carol Duvall Show (HGTV), Jewelry Making (DIY), Good Things Utah (ABC) and Beads, Baubles and Jewels (PBS).
Sherri leads numerous jewelry making workshops nationwide and has been a pioneer in the industry since 1996. She is known for tracking trends and then educating consumers about how to use new products and techniques. Sherri prominently features Smooth-On products in her books and workshops including OOMOO® 30 silicone molding rubber, Equinox® 40 silicone putty, Smooth-Cast® 300 & 325 casting resins, a variety of So-Strong® Urethane pigments, and Cast Magic® powders.
To learn more about Sherri Haab visit her website at http://www.sherrihaab.com/
(Pictures and information printed with the express permission of Sherri Haab)
Materials Used in this Tutorial
- Sulfur Free Clay
- Glue
- OOMOO® 30
- Mixing Sticks
- Mixing Containers
- Smooth-Cast® 325
- So-Strong Colorants
Step 1: Creating and Preparing Beads.
Begin by useing clay to create the shape for the bead. Then, arrange the clay shapes and glue them to the bottom of the container.
Step 2: Molding and Demolding of OOMOO™ 30
Mix OOMOO™ 30 silicone mold rubber and pour it into the container. Once the OOMOO™ 30 has cured, remove it from the container and also remove the clay shapes from the mold.
Step 3: Casting and Demolding with Smooth‑Cast® 325
Mix Smooth-Cast® 325 plus So-Strong® Red and place into a small squirt bottle. Then, put the resin into the mold cavities. When cured, remove the Smooth-Cast® 325 beads from the OOMOO® 30 mold.
Step 4: Finished Product
The beads are sanded and strung together to create these orginial bracelets.