Skin Tite®

Skin Tite®

SkinTite®为皮肤安全硅胶,用于制作快速伤口、疤痕并将硅胶装置直接粘附在皮肤上。它可以在“空中”雕刻,提供最大限度的控制和放置位置的精确性。Skin Tite®会粘附在皮肤上,并且完美地贴合所有轮廓。固化后硅胶坚固并随身体运动而弯曲。伤口和装置直到将它们去除才会脱落。材料皮肤安全并由独立实验室通过OECD TG 439和ISO 10993-10认证。
 
使用Silc Pig®硅胶颜料可以获得无限颜色效果。添加到Skin Tite®中的SilcPig®颜料将形成超逼真的切割、疤痕、砍伤、瘀伤、坏死(死皮)效果,弹孔和更多颜色效果。Thi-vex®增稠剂可增强Skin Tite®的垂直悬挂控制,适用于制作皮肤口袋、悬挂皮肤、深层切口和伤口、孔洞和更多。
 
生物粘合剂:Skin Tite®也可用于粘贴皮肤效果硅胶装置或硅胶面膜到皮肤上,即使在难以固定的区域,如肘部、手指和关节上。也适用于重复运动应用场合。Skin Tite®可以从浓密毛发覆盖的皮肤表面脱模(手臂短毛发、胡须和眉毛)

特征

说明

Store and use all products at room temperature (72° F / 22°C). This product has a limited shelf life and should be used as soon as possible.
 

We recommend that you do a small scale test on the back of your hand to ensure that you have no allergic reaction to silicone. If you notice any type of skin reaction, do not use product.

Important: Warmer temperatures will reduce pot life and accelerate the cure time of Skin Tite®.

Skin Tite® is a platinum-cure silicone. Platinum-cure silicone rubber may be inhibited by certain contaminants such as latex, skin oils, aloe vera, sulfur based clays, urethane rubber and tin-cured silicone rubber resulting in tackiness at the mold interface or a total lack of cure throughout the piece. If compatibility between the rubber and a surface is a concern, a small-scale test is recommended.Inhibition has occurred if the rubber remains uncured after the recommended cure time has passed.

Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.


Adding Color - Silc Pig ® silicone pigments can added and mixed thoroughly into Skin Tite® for matching a skin color, etc.

Mixing - Skin Tite® can be hand mixed. Aggressively hand mix for 30 seconds, making sure that you scrape the sides and bottom of your mixing container several times.

1. Using As A Bio-Adhesive - Skin Tite® can be used to temporarily adhere a previously made platinum silicone prosthetic appliance to human skin.

Here’s How To Do It: Clean the skin to remove any oils which may affect the curing of the Skin Tite® adhesive. Mix the Skin Tite® thoroughly (1A:1B). After mixing, brush a small amount of Skin Tite® onto the appliance or surface of the skin. Hold the appliance to the skin until the Skin Tite® is cured. This should occur in approximately 5 minutes or less, dependant on body temperature. A higher temperature will cause the Skin Tite® to cure faster. Once the Skin Tite® is cured, it will remain tacky. Use a small amount of Skin Tite® to carefully blend the edges of the appliance if needed. After Skin Tite® is fully cured, theatrical makeup can be used to further blend and color the piece. To remove the appliance from the skin, slowly peel the piece away from the skin. Using baby oil or make-up remover can assist in removal.

2. Using To Make Appliances Directly On The Skin - Skin Tite® can be combined with Silc-Pig® silicone pigments and a small amount of Thi-Vex® thixotropic additive to create on skin silicone appliances.

Here’s How To Do It: Mix the Skin Tite® 1A:1B by weight or volume as normal, add a small amount of pigment and mix again. After the desired color is achieved, add a small amount of Thi-vex® and continue mixing until the desired thickness is achieved. The Skin Tite® can now be applied directly to the skin to create scars, cuts, and other appliances. Use a small brush dipped in alcohol to feather the edges of the appliance. After the appliance is fully cured, theatrical makeup can be used to further blend and color the piece. To remove the appliance from the skin, slowly peel the piece away from the skin. Using baby oil or make-up remover can assist in removal.

Hair Covered Skin Surfaces - Skin Tite® will release from closely cropped hair-covered skin surfaces (short arm hair, beards, moustaches and eyebrows). If hair is too long, it will become encapsulated in rubber and careful cutting of the hair may be necessary to remove.

3. Using Skin Tite® To Cast Into A Mold To Make An Appliance - Skin Tite® can be combined with Silc-Pig® silicone pigments and poured into a mold which will create a re-useable silicone appliance.

Here’s How To Do It: You can cast Skin Tite® into either a platinum silicone mold or a rigid plaster mold. Apply a soap solution (1 part dish soap to 2 parts isopropyl alcohol works well) as a mold release and let dry at least 30 minutes. Mix Skin Tite® 1A:1B by weight or volume and cast into the mold. After the casting is fully cured, the mold release should be washed off with warm water and allowed to dry. Skin Tite® can be used to temporarily adhere the piece to the skin. Theatrical makeup can be used to further blend and color the piece. After use, remove the piece slowly. Using baby oil or makeup remover can assist in removal.