One Step™

One Step ™为方便、经济的液体密封剂和脱模剂二合一。低气味、低粘度配方作为使用Smooth-On聚氨酯模具橡胶在模具制造过程中使用封闭剂,再使用脱模剂的“一次”替代品。One Step ™将有助于石膏、混凝土、石材,砖、大理石、石灰石、木材、金属和其他从固化的聚氨酯模具橡胶和其它表面脱模。不能在模型粘土上使用

特征


说明

Safety - Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk. Use in low humidity environments. High humidity will slow evaporation of solvents. Application surface should be clean, dust free and dry. Shake container well before each use.

Store and use material at room temperature (73°F/23°C).


How To Apply - Use a dry brush to apply thorough thin coating of One Step™ over entire surface of model and any surfaces that will contact the mold rubber. Brush into deep detail and undercuts on the model.

Do not allow to pool. Blow off excess with compressed air. Let dry 15 minutes. Apply a second coating and let dry 30 minutes. Mix and apply urethane rubber as directed by the rubber product technical bulletin.

Note: if sealing an extremely porous surface (such as pressed brick), apply 3 coats of One Step™ before applying mold rubber.

Because no two applications are the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.