Black Cat™ 85

BlackCat™85为双组分快速固化液体粘合剂,用于修补钢/织物绳式橡胶输送带上的孔洞、撕裂和裂缝,具有高耐磨性和耐磨损性。还在各种基材之间提供牢固、柔性粘合,包括石膏、木材、水泥、石材、玻璃、硬塑料和各种金属。
 
在室温下(73°F /23°C),工作时间为3.5分钟,固化时间为2.5小时。

特征

说明

PREPARATION...
 

Safety - Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk.
Store and use material at room temperature (73°F/23°C). This product has a limited shelf life and should be used as soon as possible.

Conveyor Belt Repair - ensure that area to be repaired is free of grease, dirt, or moisture. Clean surface using a solvent. Approved solvents include (acetone, xylene, alcohol). Abrade surface to be bonded using an abrasive wheel or grinding disc. For holes, make sure to use duct tape to bridge holes and prevent adhesive leakage. Blow off any dust using oil-free compressed air. Clean the surface one more time using a solvent.
After mixing, apply the material using a spatula or flat edge tool as quickly as possible as it sets quickly. It is better to mix small amounts and add more material as needed. Partially cured material applied to the surface will not create a bond with suitable physical properties. A plastic spatula or a flat edged tool, are best methods for applying the material over a larger surface.

Surface Preparation for Bonding Applications - It is essential that the surface of both substrates to be bonded be absolutely clean and dry. Porous surfaces should be sanded until clean and any excess dust removed thoroughly. Non-porous surfaces should be degreased, dried and abraded by sanding, sandblasting or chemical etching - the etching being required for certain surfaces. Solvent wash the surface and let the solvent fully dry before applying adhesive.


MEASURING & MIXING...
Stir Part A and Part B thoroughly before dispensing. After dispensing equal amounts of Parts A and B into mixing container, mix thoroughly for 30 - 45 seconds making sure that you scrape the sides and bottom of the mixing container several times.


APPLYING, CURING & PERFORMANCE...
Pour on to prepared surface. Level (scrape off excess) using a spatula or flat edge tool. Position and affix other surface to substrate and clamp together for 2.5 hours at 73°F/23°C . Using in warm environments will reduce pot life and cure time. Cure time can be reduced by applying mild heat.