PREPARATION - Failure to follow directions may result in the urethane system not curing or not attaining ultimate physical and performance

properties. Follow safety precautions listed on the urethane material technical bulletin and SDS. Store and use allmaterials at room temperature (73°F/23°C).

MEASURING & MIXING - To use, add 0.25 grams (10 drops) of Doxy 5® for every 1 lb. / 0.5 kg. of material.

Add Doxy 5® to the Part B side of any urethane resin system and pre-mix. Combine with Part A, mix thoroughly and
vacuum material. Doxy 5® will significantly reduce the amount of time it takes to vacuum the mixture.

This product has a limited shelf life and should be used as soon as possible.