MEASURING & MIXING
 

How Much To Add? - To get you started, we offer the following loading level recommendation. Results may vary.

By Weight Using A Gram Scale: 1 part for every 100 parts of mixed material (A+B).

By Volume Measured In Drops: Add 5 drops of Cryptolyte® per 3 oz (88 ml) of mixed silicone or urethane material (A+B).

Important: Best “glow” effect is realized when Cryptolyte® is added to clear (i.e. Sorta Clear® silicone or Clear Flex® urethane rubber) or translucent materials (i.e. Smooth-Cast® 325 resin).

Applications Include - special effects, Halloween mask and prop making, theme displays and security (you can make parts that are virtually undetectable in normal light but glow under UV black lighting).

Warning: This product is flammable. Exercise extreme caution and follow safety protocol for handling flammable liquids. Refer to MSDS for further safety information.