Overview
In this tutorial we show how FlexFoam-iT! 15 can be used to repair a damaged John Deere® tractor seat. FlexFoam-iT!™ 15 is a unique formulation which has a relatively long, 2 minute pot life. FlexFoam is part of our “Tuff Stuff” line, which is formulated for exceptional strength.
Materials Used in this Tutorial
FlexFoam-iT! 15 "Tuff Stuff"
Mixing Cups
Stirring Stick
Plastic Syringe
Painters' Tape
Step 1: Identify Areas to Repair
The foam seat of this tractor has extensive damage at the seam and inner filling. Injecting foam into the damaged area will increase comfort and close the gap at the seam.
Step 2: Measure and Mix FlexFoam-iT! 15 Tuff Stuff
FlexFoam-iT! 15 is mixed 1A:2B by volume or 100A:185B by weight using an accurate gram scale. A small amount of material is dispensed by weight then stirred quickly and deliberately for 15 seconds, making sure to aggressively scrape the sides and bottom of the mixing container several times.
Step 3: Apply Foam to Repair
The two minute pot life allows for the liquid foam to be drawn into a plastic syringe for dispensing into the damaged area of the foam. Foam is injected at multple spot along the seam then painters' tape is used to hold the cushion together.
Step 4: The Repair is Complete
After four hours, the tape is removed and the seat cushion is examined–a perfect repair! The seat is reinstalled on the tractor and is ready for use.