Instructions

Safety - Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk. Wear vinyl gloves only. Latex gloves will inhibit the cure of the rubber. Store and use material at room temperature (73°F/23°C). Warmer temperatures will drastically reduce working time and cure time. Storing material at warmer temperatures will also reduce the usable shelf life of unused material. These products have a limited shelf life and should be used as soon as possible.

Cure Inhibition - Addition cured silicone rubber may be inhibited by certain surface contaminants. If surface compatibility is in question, do a small compatibility test before using for an important project.

MEASURING & MIXING...

Mixing by Hand - Before you begin, pre-mix Part B thoroughly. After dispensing required amounts of Parts A and B into mixing container (1A:1B by volume or weight), mix thoroughly by hand or using a turbine mixer (available at your local Smooth-On distributor). Material should be mixed for 3 minutes before pouring, making sure that you scrape the sides and bottom of the mixing container several times.

APPLYING & CURING...

Applying by Hand - Apply a uniform layer across all surfaces using a scraper tool or brush. If applying in layers (approximately 0.06” / 1.5mm per layer), let the first coat cure for 3 hours at room temperature until material becomes “tacky” before adding the next coat. Repeat until the necessary thickness is achieved.

Meter Mix Dispensing - Si-Tac™ Parts A and B are meter mix dispensed and delivered to the garment surface at strategic points through a narrow static mixing tube. The garment is then run through a heat tunnel and exposed to 200°F / 94°C or higher so that the silicone cures in 1 minute or less. For information on meter mix equipment, contact Smooth-On or your nearest Smooth-On distributor.

Curing - Let silicone cure 6 hours at 73°F / 23°C.

Heat Curing - Cure time can be reduced to under 1 minute by applying heat (200°F / 94°C).