Body Double™ Fast Set

Body Double™ Fast Set vs. Body Double™ Standard Set vs. Body Double™ Silk

Fast Setting “Apply to Skin” Platinum Silicone Rubber

› View Product

Vs.
remove

Body Double™ Standard Set

Body Double™ Fast Set vs. Body Double™ Standard Set vs. Body Double™ SilkBody Double™ Fast Set

Medium Setting “Apply to Skin” Platinum Silicone Rubber

› View Product

Vs.
remove

Body Double™ Silk

Body Double™ Fast Set vs. Body Double™ Standard Set vs. Body Double™ SilkBody Double™ Fast Set versus Body Double™ Standard Set

Self-Releasing Lifecasting Silicone Rubber

› View Product

Add Material to Compare

start over

Key Differences

Pot Life90 seconds5 minutes6 minutes
Cure Time7 minutes20 minutes20 minutes
Specific Volume23.7 cu. in./lb.23.7 cu. in./lb.30.4 cu. in./lb.
ColorAqua, GreenPurpleGreen
Disclaimer
Although we do our best to ensure the accuracy of this Compare Tool, Smooth-On offers no warranty either expressed or implied as to the reliability of the information contained herein. Smooth-On assumes no liability for loss or damage associated with use of the Compare Tool. If this is a critical project, we encourage you to review all of the technical data below and contact our Technical Service department with any questions or concerns.

All Technical Data

Body Double™ Fast SetBody Double™ Standard SetBody Double™ Silk
Product Type
  • Silicone Rubber - Platinum Cure
  • Lifecasting Materials
  • Silicone Rubber - Platinum Cure
  • Lifecasting Materials
  • Silicone Rubber - Platinum Cure
  • Lifecasting Materials
Mixed ViscosityBrushableBrushableBrushable
Mix Ratio By Volume1A:1B1A:1B1A:1B
Mix Ratio By Weight1A:1B1A:1B1A:1B
Pot Life90 seconds5 minutes6 minutes
Cure Time7 minutes20 minutes20 minutes
Shore A Hardness252525
Specific Gravity1.17 g/cc1.17 g/cc0.91 g/cc
Specific Volume23.7 cu. in./lb.23.7 cu. in./lb.30.4 cu. in./lb.
ColorAqua, GreenPurpleGreen
Die C Tear Strength40 pli40 pli—
Tensile Strength450 psi525 psi—
Elongation @ Break500 %500 %—
Shrinkage<.001 in. / in.<.001 in. / in.<.001 in. / in.

Product Description

Body Double™ Fast Set

Body Double™ is a long lasting platinum-cure silicone rubber that can be applied directly to the skin to make molds of the face, hands and other body parts. The rubber cures quickly and will reproduce perfect detail from any original model – far better detail than any alginate!

›Read More

Body Double™ Standard Set

Body Double™ is a long lasting platinum-cure silicone rubber that can be applied directly to the skin to make molds of the face, hands and other body parts. The rubber cures quickly and will reproduce perfect detail from any original model – far better detail than any alginate!

›Read More

Body Double™ Silk

Body Double™ SILK is a self-releasing platinum-cure silicone rubber that can be applied directly to the skin to make molds of the face, hands and other body parts. The rubber cures quickly and will reproduce excellent detail from any original model.

Body Double™ SILK will release from closely cropped hair-covered skin surfaces(short beards, mustaches, eyebrows, pubic hair, etc.). Release cream or Hyperfolic are not needed when using Body Double™ SILK. Body Double™ SILK will last for many castings of almost any material including plaster, Matrix™ Neo™, wax, resins (Smooth-Cast urethanes, polyester, etc.) Body Double™ SILK has a working time of 6 minutes and a demold time of 20 minutes*.

*Depending on material temperature, ambient temperature and body temperature – see “Preparation” below for details.

›Read More