Key Differences

Pot Life30 minutes45 minutes
Shore A Hardness00-2000-30
Die B Tear Strength30 pli38 pli
Disclaimer
Although we do our best to ensure the accuracy of this Compare Tool, Smooth-On offers no warranty either expressed or implied as to the reliability of the information contained herein. Smooth-On assumes no liability for loss or damage associated with use of the Compare Tool. If this is a critical project, we encourage you to review all of the technical data below and contact our Technical Service department with any questions or concerns.

All Technical Data

Ecoflex™ 00-20Ecoflex™ 00-30
Product Type
  • Silicone Rubber - Platinum Cure
  • Silicone Rubber - Platinum Cure
Mixed Viscosity3,000 cps3,000 cps
Mix Ratio By Volume1A:1B1A:1B
Mix Ratio By Weight1A:1B1A:1B
Pot Life30 minutes45 minutes
Cure Time4 hours4 hours
Shore A Hardness00-2000-30
Specific Gravity1.07 g/cc1.07 g/cc
Specific Volume26.0 cu. in./lb.26.0 cu. in./lb.
ColorTranslucentTranslucent
Die B Tear Strength30 pli38 pli
Tensile Strength160 psi200 psi
Elongation @ Break845 %900 %
100% Modulus8 psi10 psi
Shrinkage<.001 in. / in.<.001 in. / in.
Useful Temperature (min)-65 °F-65 °F
Useful Temperature (max)450 °F450 °F

Product Description

Ecoflex™ 00-20

Ecoflex™ rubbers are platinum-catalyzed silicones that are versatile and easy to use. Ecoflex™ rubbers are mixed 1A:1B by weight or volume and cured at room temperature with negligible shrinkage. Low viscosity ensures easy mixing and de-airing, or you can choose to mix and dispense using our convenient dispensing cartridges. Cured material is skin safe and certified by an independent laboratory to ISO 10993-10, Biological evaluation of medical devices, Part 10: Tests for irritation and skin sensitization.

Certified Skin Safe - Ecoflex™ 00-20 is skin safe and certified by an independent laboratory to OECD TG 439.

›Read More

Ecoflex™ 00-30

Ecoflex™ rubbers are platinum-catalyzed silicones that are versatile and easy to use. Ecoflex™ rubbers are mixed 1A:1B by weight or volume and cured at room temperature with negligible shrinkage. Low viscosity ensures easy mixing and de-airing, or you can choose to mix and dispense using our convenient dispensing cartridges. Cured material is skin safe and certified by an independent laboratory to ISO 10993-10, Biological evaluation of medical devices, Part 10: Tests for irritation and skin sensitization.

›Read More