Key Differences

Product Type
  • Silicone Rubber - Tin Cure
  • Silicone Rubber - Platinum Cure
Mixed Viscosity14,000 cps23,000 cps
Mix Ratio By VolumeN/A (gram scale required)1A:1B
Pot Life45 minutes8 minutes
Cure Time24 hours75 minutes
Elongation @ Break586 %1,000 %
100% Modulus29 psi22 psi
Disclaimer
Although we do our best to ensure the accuracy of this Compare Tool, Smooth-On offers no warranty either expressed or implied as to the reliability of the information contained herein. Smooth-On assumes no liability for loss or damage associated with use of the Compare Tool. If this is a critical project, we encourage you to review all of the technical data below and contact our Technical Service department with any questions or concerns.

All Technical Data

Mold Max™ 10TDragon Skin® 10 FAST
Product Type
  • Silicone Rubber - Tin Cure
  • Silicone Rubber - Platinum Cure
Mixed Viscosity14,000 cps23,000 cps
Mix Ratio By Volume—1A:1B
Mix Ratio By Weight100A:10B1A:1B
Pot Life45 minutes8 minutes
Cure Time24 hours75 minutes
Shore A Hardness1010
Specific Gravity1.09 g/cc1.07 g/cc
Specific Volume25.4 cu. in./lb.25.8 cu. in./lb.
ColorTranslucentTranslucent
Die B Tear Strength87 pli102 pli
Tensile Strength405 psi475 psi
Elongation @ Break586 %1,000 %
100% Modulus29 psi22 psi
Shrinkage0.0025 in. / in.<.001 in. / in.
Useful Temperature (min)-65 °F-65 °F
Useful Temperature (max)400 °F450 °F

Product Description

Mold Max™ 10T

Mold Max™ 10T silicone is a water white translucent tin cured silicone rubber compound that has exceptional tear strength and working properties. It features Smooth-On’s “Libra™” catalyst for long library life. Mixed 100A:10B by weight, vacuum degassing is recommended for de-airing. Rubber cures overnight at room temperature. Mold Max™ ‘T’ silicones can be thickened with Thi‑Vex™ thickener for brush-on application and effects.

›Read More

Dragon Skin® 10 FAST

Dragon Skin® silicones are high performance platinum cure liquid silicone compounds that are used for a variety of applications ranging from creating skin effects and other movie special effects to making production molds for casting a variety of materials. Because of the superior physical properties and flexibility of Dragon Skin® rubbers, they are also used for medical prosthetics and cushioning applications. Dragon Skin® rubbers are also used for a variety of industrial applications and have a service temperature range of a constant -65°F to +450°F (-53°C to +232°C)