Compare Tool

remove

Mold Max™ 30

Mold Max™ 30 vs. OOMOO™ 30

High Performance Silicone Rubber

› View Product

Vs.
remove

OOMOO™ 30

Mold Max™ 30 vs. OOMOO™ 30Mold Max™ 30

No Scale or Vacuum Chamber Required

› View Product

Add Material to Compare

start over

Key Differences

Mixed Viscosity25,000 cps4,250 cps
Mix Ratio By VolumeN/A (gram scale required)1A:1B
Pot Life45 minutes30 minutes
Cure Time24 hours6 hours
ColorPinkLavender
Die B Tear Strength125 pli40 pli
Tensile Strength577 psi240 psi
Disclaimer
Although we do our best to ensure the accuracy of this Compare Tool, Smooth-On offers no warranty either expressed or implied as to the reliability of the information contained herein. Smooth-On assumes no liability for loss or damage associated with use of the Compare Tool. If this is a critical project, we encourage you to review all of the technical data below and contact our Technical Service department with any questions or concerns.

All Technical Data

Mold Max™ 30OOMOO™ 30
Product Type
  • Silicone Rubber - Tin Cure
  • Silicone Rubber - Tin Cure
Mixed Viscosity25,000 cps4,250 cps
Mix Ratio By Volume—1A:1B
Mix Ratio By Weight100A:10B100A:130B
Pot Life45 minutes30 minutes
Cure Time24 hours6 hours
Shore A Hardness3030
Specific Gravity1.18 g/cc1.34 g/cc
Specific Volume23.5 cu. in./lb.20.6 cu. in./lb.
ColorPinkLavender
Die B Tear Strength125 pli40 pli
Tensile Strength577 psi240 psi
Elongation @ Break300 %250 %
100% Modulus110 psi—
Shrinkage0.002 in. / in.0.0025 in. / in.
Useful Temperature (min)-65 °F-65 °F
Useful Temperature (max)400 °F400 °F

Product Description

Mold Max™ 30

Mold Max™ Silicones are tin-cured silicone rubber compounds that have exceptional working properties and library life. Mold Max™ Silicones feature Smooth-On’s exclusive “Libra™” catalyst for long library life. Mold Max™ silcones can be pigmented with Silc Pig™ silicone colorants. Pot life for the pourable silicones is 45 minutes and they cure overnight at room temperature.

Vacuum degassing mixed material using a vacuum pump and chamber to remove entrapped air is recommended.

›Read More

OOMOO™ 30

No Vacuuming – No Scale – Easy To Use . . . OOMOO™ 30 is an easy to use silicone rubber compound that features a convenient one-to-one by volume mix ratio (no scale necessary). It has low viscosity for easy mixing and pouring . . . vacuum degassing is not necessary. This product cures at room temperature with negligible shrinkage. OOMOO™ 30 has a 30-minute pot life, with a six-hour cure time.

For The Novice Mold Maker - OOMOO™ silicones do not have great tear strength. They are good for making simple one- or twopiece block molds. If you require a high-tear strength silicone, Mold Max™ silicones are recommended.

OOMOO™ 30 is suitable for a variety of art-related and industrial applications including making one and two-piece block molds for sculpture and prototype reproduction, casting plaster, resins and wax. OOMOO™ silicones are also suitable for electrical potting and encapsulation applications.

›Read More